Effect of operating temperature on creep and damage in the bonded compliant seal of planar solid oxide fuel cell
ترجمه فارسی عنوان
اثر دمای کار بر روی خزش و آسیب در مهر و موم سازگار پیوند سلول سوخت اکسید جامد مسطح
کلمات کلیدی
موضوعات مرتبط
مهندسی و علوم پایه شیمی الکتروشیمی
چکیده انگلیسی
This paper studies the effect of operating temperature on creep and damage in bonded compliant seal of solid oxide fuel cell by finite element method. A strain based creep damage model is used, and its feasibility to predict the creep damage behavior of the materials is verified firstly by the experimental data. The results show that the failure locates at the foil and the location varies with the temperature increasing. When the temperature is lower than 600 °C, there is nearly no crack occurs. When the temperature is 600 °C, the creep crack belongs to internal crack and the length is about 2.5 mm. While the temperature is 650 °C or higher, the crack locates at the foil surface and the length is larger than 25 mm at an operation time of 50,000 h. Compared to the size of the whole structure, an internal crack of 2.5 mm is small and the gas leakage will not happen. Therefore, it can satisfy the requirement of safe operation for more than 40,000 h. Thus, it recommends that the operating temperature should not be higher than 600 °C on the condition of insuring the power performance and operation cost of the SOFC.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: International Journal of Hydrogen Energy - Volume 43, Issue 9, 1 March 2018, Pages 4492-4504
نویسندگان
, , , , ,