This paper reports on the interfacial reaction kinetics between molten Sn–58Bi solder and Cu substrates for extended temporal scales. Also studied are the effects of a series of elemental additions of 1–2 wt.% Al, Cr, Cu, Si, Zn, Ag, Au, Pt and Nb into the basic Sn–58Bi solder, in an attempt to produce a barrier layer that slows down intermetallic compound (IMC) growth. At temperatures between 200 and 240 °C, grain boundary-/molten channel-controlled growth of η-phase (Cu6Sn5), followed by diffusion-controlled simultaneous growth of the ε-phase (Cu3Sn) and η-phase (Cu6Sn5), between the molten Sn–58Bi solder and the Cu substrate was observed, and a layer of 6 μm Cu could survive for approximately 24–48 h. Addition of 1 wt.% Zn resulted in a layer of γ-Cu5Zn8, instead of Cu3Sn and Cu6Sn5, forming at the interface, leading to an increase in the lifetime of the Cu substrate to greater than 120 h at 200 °C, while the other additions failed to slow down IMC formation.
Journal: Acta Materialia - Volume 54, Issue 11, June 2006, Pages 2907–2922