Chromium sesquioxide (Cr2O3) nanoparticles have been successfully synthesized via the facile solvothermal process, by using CrO3 in different solvents. The as-synthesized nanoparticle sizes are calculated and confirmed to be 25–45 nm, by using X-ray diffraction (XRD) and transmission electron microscopy (TEM). The functional groups of the samples were tested by the Fourier transform infrared (FTIR) spectroscopy. Fine and spherical-like morphologies and compositional elements of the products were observed by the scanning electron microscopy (SEM) and energy dispersive X-ray (EDX) spectroscopy. A weak ferromagnetic (WFM) property was observed for sample by the vibrating sample magnetometer (VSM). The observed band gap values (Eg=4.33–3.54 eV) higher than that of bulk Cr2O3 (~3.4 eV) indicated that the particles had been successfully synthesized in the nano region, and measured by ultra-violet visible (UV–vis) absorption spectroscopy. The broad visible emission at ~399 nm, in the photoluminescence spectroscopy revealed the high purity and perfect crystallinity of the samples.
Journal: Materials Science in Semiconductor Processing - Volume 19, March 2014, Pages 136–144