Improved luminescence properties of nanocrystalline silicon based electroluminescent device by annealing
چکیده انگلیسی
We report an annealing effect on electrical and luminescence properties of a red electroluminescent device consisting of nanocrystalline silicon (nc-Si). The red luminescence was generated by flowing the forward current into the device at a low threshold direct current (DC) forward voltage with a rise of annealing temperature up to 500 °C. Moreover, the luminescence of the device annealed at 500 °C was more intense than that of the device annealed at 200 °C or less under the same forward current density, because of the injection of a large quantity of carriers to the radiative recombination centers at the nc-Si surface vicinity. These were attained by a low resistivity of indium tin oxide (ITO) electrode and good contact at the ITO electrode/luminous layer interface region by the annealing treatment. The above results indicated that the annealing treatment of the device is effective for the realization of high luminance due to the improvement in the injection efficiency of carriers to the radiative recombination centers.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Thin Solid Films - Volume 515, Issue 2, 25 October 2006, Pages 778-781
نویسندگان
, ,