An analysis of the Portevin-Le Chatelier effect and cracking of CuSn6P alloy at elevated temperature of deformation applying the acoustic emission method
Keywords: فرکتوگرافی یا ریخت شناسی; Copper alloy; Portevin-Le Chatelier phenomenon; Fractography; Acoustic emission; Intercrystalline fracture;