Artificial Neural Network (ANN) based microstructural prediction model for 22MnB5 boron steel during tailored hot stamping
Keywords: دندانه گذاری نانو; Artificial Neural Network; Tailored hot stamping; Microstructure; Nanoindentation; 22MnB5 boron steel; Modelling;